by Lori Jo Vest | Jun 26, 2025 | Blog
This Issue: We’re spotlighting the evolution of Press Hardening Steel Grades, from the original 22MnB5 to today’s cutting-edge grades, and sharing practical solutions for joining AHSS. Whether you’re engineering for performance or production,...
by Lori Jo Vest | May 29, 2025 | Blog, General News
As the automotive industry transforms to future mobility, safety will remain a top priority. WorldAutoSteel’s Steel E-Motive (SEM) concept vehicle demonstrates how Advanced High-Strength Steels (AHSS) can meet the most demanding global crash requirements, even in...
by Lori Jo Vest | Nov 26, 2024 | Blog, General News
Liquid Metal Embrittlement (LME) surface cracks may develop during resistance spot welding in advanced high-strength steels used in automotive bodies. While LME mechanisms are well-documented for academic, single-spot samples, there is limited data on production-scale...
by Lori Jo Vest | Oct 22, 2024 | Blog, General News
Results of our latest study on Liquid Metal Embrittlement confirm that LME is predictable and preventable. Download the Phase 2 Report Download the Phase 1 Report In the automotive industry, ensuring the strength and safety of vehicle welds is critical. With the...
by Lori Jo Vest | Apr 23, 2024 | Blog
WorldAutoSteel advances steel’s advantages in the automotive and future mobility industries. We’re committed to engaging with future engineers at post-secondary education organizations around the globe. Our most recent engineering project, Steel E-Motive,...