In this AHSS Insights blog post Akshay Wankhede, Application Engineer at AutoForm, describes the causes for the springback phenomenon known as the “sidewall curl”, how its occurrence on stamped panels can be identified early through simulation of full production process, and how it can be counter-measured well ahead of die tryout. Read this post to understand the challenges of the sidewall curl effect for Advanced High-Strength Steels.  Join the dialogue here! >>>

 

 

 

 