High magnification photograph of a galvannealed steel surface.  The surface structure results in excellent paint adhesion.

High magnification photograph of a galvannealed steel surface. The surface structure results in excellent paint adhesion.

Many steel parts on a vehicle require corrosion protection, regardless of whether they are exposed or unexposed applications. The most common way to accomplish corrosion protection is to coat Advanced High-Strength Steels (AHSS) with zinc by means of a couple of different processes. This AHSS Insights Blog goes over the most common.  Click here read the whole article >>

 