STEEL ELIMINATES WEIGHT GAP WITH ALUMINIUM FOR CAR BODIES

New studies show a further reduction in body structure mass

FSV BEV Peel Away

The latest in a continuing series of research studies strongly suggest that steel auto body structures in the near future can be as lightweight as today’s aluminium bodies, while meeting all crash performance standards and at comparable cost of current steel structures.

The studies also address critical manufacturing challenges, showing that car makers can form and fabricate sophisticated steel designs, thus accelerating implementation of this technology into production vehicles.   Read more and download the reports>>

 