ULSAC

UltraLight Steel Auto Closures frameless door
  • 42% lighter than the average benchmarked frameless door
  • 22% lighter than the best-in-class benchmarked door (framed door)
  • 46% lighter than the average benchmarked frameless door
  • 27% lighter than the best-in-class benchmarked door (framed door)

The Ultralight Steel Auto Closure (ULSAC) Program is a study undertaken by the global steel producers to demonstrate the effective use of steel in producing lightweight, structurally sound steel automotive closures that are manufacturable and affordable. ULSAC began as a concept development program, producing lightweight designs for doors, hoods, decklids and hatches that are up to 32% lighter than the average benchmark. The program continued to the manufacture of steel frameless door demonstration hardware that achieves dramatic results in mass reduction and performance, yet is manufacturable in high-volume at affordable costs.

Click the links to learn more about ULSAC’s features and achievements.

Error: Please enter a valid email address

Error: Invalid email

Error: Please enter your first name

Error: Please enter your last name

Error: Please enter a username

Error: Please enter a password

Error: Please confirm your password

Error: Password and password confirmation do not match