Understanding Tensile Testing for Better Metal Forming Simulations
Tensile testing provides essential data for metal forming simulations, but using the wrong stress-strain model can lead to inaccurate results. Engineering stress-strain curves, based on initial...
WorldAutoSteel February 2025 Update
Updated Steel E-Motive Engineering Report Now Available An updated Steel E-Motive Engineering Report is now available for download on steelemotive.world. The latest edition features a lifecycle...
WorldAutoSteel Winter Update – Happy New Year!
2024 proved to be another important milestone year for WorldAutoSteel, with a critical focus on our mission of advancing steel solutions for future mobility and positioning steel as the material of...
WEBINAR Replay: Understanding Liquid Metal Embrittlement (LME) in Advanced High Strength Steel Components
Liquid Metal Embrittlement (LME) surface cracks may develop during resistance spot welding in advanced high-strength steels used in automotive bodies. While LME mechanisms are well-documented for...
WorldAutoSteel Publishes New Liquid Metal Embrittlement Component Study
Results of our latest study on Liquid Metal Embrittlement confirm that LME is predictable and preventable. Download the Phase 2 Report Download the Phase 1 Report In the automotive industry,...
15th Steelie Awards Winners Announced
The World Steel Association (worldsteel) has announced the winners for the 15th Steelie Awards. The Steelie Awards recognize worldsteel member companies for their contribution to the steel industry...