Background
The Super LIGHT-Car (SLC) project was initiated in 2005 by a consortium of 38 leading European organizations, with Volkswagen serving as project coordinator. It was co-funded by the European Commission under the 6th Framework Programme, and was part of the European Council for Automotive Research’s (EUCAR) multi-material development efforts. The primary goal of SLC was to develop a real, multi-material C-Class body structure (BIW) that achieved a 30% weight reduction, compared to the 2005 benchmark vehicles. Other goals included reduced material consumption, lightweighting costs of no more than 5 €/kg, equivalent structural performance, and the capability of being produced at a rate of 1,000 vehicles per day.
During the second year of the project, three vehicle concepts were developed, each with a different focus. The first was the Universal Light Body Concept (ULBC), which focused on all of the original project goals, but with a cost requirement (< 2.5 €/kg) even lower than the original goal set for the project. This effort resulted in a 29% mass reduction of 82 kg, at an additional cost of 2,7 €/kg. The second was the Super Light Body Concept (SLBC). The focus here was maximising weight saving, with a more generous cost requirement of < 10 €/kg savings. The results were a mass reduction of 41%, or 114 kg, with a cost increase of 2,70 €/kg. The third concept was developed by ArcelorMittal, one of the SLC partners, whose all-steel efforts focused achieving cost-effective weight reduction through the utilization of the latest grades of steel.
Blending these three designs into one, the Super LIGHT Car utilises a wide range of materials: 53% aluminium, 36% steel (in a variety of grades), 7% magnesium, and 4% composite.
Material distribution for SLC is shown below.
Figure 1: Super LIGHT Car material distribution
The SLC study included a cost analysis, but did not include a life cycle assessment (LCA). The analysis showed the cost to produce SLC was 112% of the reference vehicle, a Golf V. Stated differently, the cost of lightweighting in SLC was more than 7 €/kg.
Volkswagen and PE International conducted a Life Cycle Assessment (LCA) of the body structure, but appear to have apportioned use phase savings based on the weight savings from the multi-material approach. This has to the potential of greatly exaggerating use phase savings; indeed, they concluded that Use phase savings more than offset the high production emissions, and noted that “recycling credits for magnesium and aluminium were higher than the steel reference vehicle”.
Life Cycle Assessment Parameters
A vehicle Life Cycle Assessment (LCA) was conducted by WorldAutoSteel comparing the SLC to a Volkswagen Golf V as the baseline vehicle, and a simulated Golf V manufactured from AHSS. We used the UCSB Phase 2 GHG Materials Comparison Model (June 30, 2010), featuring the most up-to-date LCI’s for steel (worldsteel, 2010) and aluminium (IAI, 2005). Our vehicle analysis included an estimated lifetime mileage of 200,000 km and fuel consumption ratings of 7.2 L/100km or 32.7 mpg, Golf V performance with a 1.6 liter gasoline ICE. All evaluations were conducted with a recycling treatment consistent with end-of-life methodology, the prescription adopted by the metals industry (alpha value = 0.1). This treatment favours materials with high manufacturing emissions. The modelling parameters are shown in Table 1.
|
|||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
.
AHSS Mass Reduction Potential. The UltraLight Family of Research, as well as industry practice, shows that a 25% mass reduction can be achieved with AHSS compared to conventional mild steel. Optimisation techniques have yielded light weighting potential beyond 35% for specific sub-systems. In our AHSS-intensive Golf V concept we’ve estimated mass reduction potential of 20% compared to the baseline vehicle, recognizing the potential of optimisation and the reality of a body structure already utilising some AHSS products.
Table 2 (below) shows the results of the UCSB modelling.
.
Conclusions
- Multi-material vehicles have distinct emissions advantages in the use phase, but distinct disadvantages in the production phase. Figure 2 shows, however, that with optimal recycling behavior, Super LIGHT Car achieves slightly lower life cycle emissions compared to the AHSS-intensive concept.
- Contrary to the misperception that material production emissions are insignificant, Super LIGHT Car’s production emissions account for ~12% of its lifetime emissions, and thus cannot be ignored when considering environmental impacts. As the use of advanced powertrains (such as hybrids) and improved driving cycles (such as the implementation of timed lights and roundabouts) accelerate, dramatic reductions in use phase GHG emissions occur, and material production emissions will become a key determinant of total life cycle emissions.
.
- The AHSS-intensive Golf V concept is the only material / design solution that results in mass, cost and emission savings in all life cycle phases, compared to the baseline design.
.
- Super LIGHT Car (or multi-material vehicle), results in 65% greater production emissions compared to the AHSS-intensive concept vehicle. Accumulative emissions are thus significantly greater until recycling occurs at vehicle end-of-life. Due to concerns regarding the infrastructure for recycled content of GHG-intensive materials, the benefits from recycling of these materials is at minimum one vehicle life cycle, or 12 years, into the future. It’s important to note that a high percentage of recycling is a fundamental requirement of energy-intensive materials (magnesium and aluminium), in order to offset their production emissions. Small changes in their recycling rates will have a large impact on GHG emissions.
.
- A more realistic comparison of emissions performance for these vehicles would be to discount recycling credits altogether, until these vehicles actually demonstrate recycling behaviour that match recycling assumptions. In this scenario, Super LIGHT Car shows 650 kg greater CO2e per vehicle compared to the AHSS-intensive concept. With an assumption of 15 million vehicle production by 2015, this accounts for ~10 million additional tons of CO2e annual emissions.
.
- Research studies argue that upfront emissions cause greater damage to the environment due to Cumulative Radiative Forcing (CRF) and propose the application of a Time Correction Factor (TCF) to account for such temporal effects. AISI and UC-Davis are collaborating on a study that will provide data to legislators, emphasizing the need for LCA and CRF cumulative effects to prevent tailpipe emissions legislation that cause unintended consequences. To demonstrate the effect, Figure 3 is a chart with TCF’s applied to the material production and recycling phases of the total vehicle life cycle. The results demonstrate the difficulty in recovering from the harmful emissions associated with environmentally unfriendly materials.
- Present literature describing emissions allocated to the Body Structure (BIW) leads to an overestimation of the fuel consumption impact of vehicle mass reduction, and “is just plain wrong” (Dr. Geyer, UCSB Bren School of Environmental Science).