New AHSS Guidelines Support Use of the Latest, Lightest Steel Technologies

AHSS Application Guidelines

Advanced High-Strength Steels Application Guidelines V5.0 combines metallurgy, forming and joining experiences from around the world

Livonia, Mich., May 14, 2014 – Today at the Great Designs in Steel automotive conference, WorldAutoSteel announced the launch of the Advanced High-Strength Steels Application Guidelines (AHSS Guidelines) Version 5.0, the largest and most comprehensive update since its first publication in 2004.

WorldAutoSteel offers the AHSS Guidelines free of charge at worldautosteel.org, to aid automakers and manufacturers in applying the latest in lightweight steels.  Read more and Get the Guidelines>>>