Dual Phase (DP) Steels

DP steels consist of a ferritic matrix containing a hard martensitic second phase in the form of islands. Increasing the volume fraction of hard second phases generally increases the strength. DP (ferrite plus martensite) steels are produced by controlled cooling from the austenite phase (in hot-rolled products) or from the two-phase ferrite plus austenite phase (for continuously annealed cold-rolled and hot-dip coated products) to transform some austenite to ferrite before a rapid cooling transforms the remaining austenite to martensite.

Depending on the composition and process route, hot-rolled steels requiring enhanced capability to resist stretching on a blanked edge (as typically measured by hole expansion capacity) can have a microstructure containing significant quantities of bainite.
 
Figure 1-2 shows a schematic microstructure of DP steel, which contains ferrite plus islands of martensite. The soft ferrite phase is generally continuous, giving these steels excellent ductility. When these steels deform, strain is concentrated in the lower-strength ferrite phase surrounding the islands of martensite, creating the unique high work-hardening rate exhibited by these steels.
 
Dual Phase (DP) Steel

Figure 1-2 - Schematic shows islands of martensite in a matrix of ferrite.
 

The work hardening rate plus excellent elongation creates DP steels with much higher ultimate tensile strengths than conventional steels of similar yield strength. Figure 1-3 compares the engineering stress-strain curve for HSLA steel to a DP steel curve of similar yield strength. The DP steel exhibits higher initial work hardening rate, higher ultimate tensile strength, and lower YS/TS ratio than the similar yield strength HSLA. Additional engineering and true stress-strain curves for DP steel grades are located in the AHSS Application Guidelines, Figure 2-9B.
 

Figure 1-3 - The DP 350/600 with higher TS than the HSLA 350/450
 

DP and other AHSS also have a bake hardening effect that is an important benefit compared to conventional higher strength steels. The bake hardening effect is the increase in yield strength resulting from elevated temperature aging (created by the curing temperature of paint bake ovens) after prestraining (generated by the work hardening due to deformation during stamping or other manufacturing process). The extent of the bake hardening effect in AHSS depends on the specific chemistry and thermal histories of the steels. Additional bake hardening information is located in AHSS Application Guidelines Section 2.C.1.g. 

In DP steels, carbon enables the formation of martensite at practical cooling rates by increasing the hardenability of the steel. Manganese, chromium, molybdenum, vanadium, and nickel, added individually or in combination, also help increase hardenability. Carbon also strengthens the martensite as a ferrite solute strengthener, as do silicon and phosphorus. These additions are carefully balanced, not only to produce unique mechanical properties, but also to maintain the generally good resistance spot welding capability. However, when welding the highest strength grade (DP 700/1000) to itself, the spot weldability may require adjustments to the welding practice.
 
 
 
Bookmark and Share

8 Comments
First  |  Previous  |  Next  |  Last
Posted by vijaya.svsmmt2002 on Jul 1 2010 5:28AM
Nice information about DP and i want more information on it,
in continous Casting how dp will be developed and what type of conditions needed.
Posted by admin on Jul 5 2010 10:26AM
Continuous casting of dual-phase steels is not much different from other steel grades. The main difference between low-carbon steels and dual-phase steels should be found in its composition and the heat treatment cycle; this will give it its particular microstructure. For more information on steel processing, please see the steeluniversity.org website: http://www.steeluniversity.org/content/html/eng/default.asp?catid=3&pageid=650269858.
Posted by admin on Jul 5 2010 10:27AM
As for further developments in the area of dual-phase steels, steel companies are working on dual phase materials with higher strength levels (up to 1280 MPa) and higher ductility levels (up to 20%). Another development in this area is the so-called complex phase material (http://www.worldautosteel.org/SteelBasics/Steel-Types/Complex-Phase.aspx), giving better performance in bending and flanging (hole expansion) operations.
Posted by Niranjan Behera on Oct 7 2010 1:49AM
Rite.. There is no difference between DP/TRIP and HSLA/Low carbon Steel with respect to Continuous Casting.
Posted by Scanstrip on Apr 21 2011 5:14AM
Hi all,

Can any one name replacement DP steel for example what is the equivalent to DOCOL 800DP??

Regards,
Alex
Posted by arslaan70 on Aug 7 2011 6:50PM
this is really elp full for me i m the new one who enter in the steel industry and this site is really really help full for me
Posted by Briana on Oct 2 2011 12:16PM
Hi, I need help with an experiment. Given a steel with f/p structure, HR, cooled then CR 60%. We had to make 2 60s HT's then WQ. We are trying to observe why carbon in austenite really comes from right to left not left to right as expected w/ presence of p. Any thoughts?
Posted by anirudh on Nov 20 2011 4:20AM
This site has been very useful to me :)
what is the composition of dual phase & trip steel ? (% of all alloying elements)
First  |  Previous  |  Next  |  Last
Please sign in below to post a comment:
User Name:
Password:
 
Or, click here to create a FREE user account.