High Strain Rate Recommended Test Procedure

Dynamic tensile testing of sheet steels is becoming more important due to the need for more optimized vehicle crashworthiness analysis in the automotive industry. Positive strain rate sensitivity, i.e., strength increases with strain rate, offers a potential for improved energy absorption during a crash event. Different types of testing techniques have been used to generate data under dynamic conditions, each serving a specific range of strain rates and providing a specific type of information. Servo-hydraulic system, tensile Split Hopkinson Bar (SHB) system, compression Split Hopkinson Bar system, Single Bar (SB) system and drop weight systems are some of the techniques commonly used. New systems also have been developed in recent years to meet the increasing demand for dynamic testing.

However, no guidelines are available as to the testing method, specimen dimensions, measurement devices, and other important issues which are critical to the quality of testing results. As a result, data from different laboratories are often not comparable. Quality of the testing data is, in general, not satisfactory. Signal damping and curve smoothing are often necessary to make the testing data usable.

With the increasing needs for tensile steel stress-strain data at dynamic conditions, WorldAutoSteel pursued the development of a Recommended Practice for Dynamic Tensile Testing for Sheet Steels. A team composed of testing experts from WorldAutoSteel steel company members was commissioned in March 2003 to pursue this developmental work and ultimately draft the recommended practice. Data on the sheet steel experiences of major testing laboratories were compiled, including ArcelorMittal, Colorado School of Mines, Ispat Inland Inc., JFE, Nippon Steel Corporation, POSCO, Sumitomo Metals, Technical University of Aachen, ThyssenKrupp Stahl, University of Dayton Research Institute and University of California at San Diego.

After a draft recommended practice was developed, a Round Robin test program was launched in early 2004 and completed in early 2005. Based on the results from the Round Robin test program, the recommended practice was modified and the specimen geometry was further refined.

The final Recommended Practice for Dynamic Tensile Testing for Sheet Steels includes information on the scope of the project, some specifics about high strain rate testing, machine types and input methods, specimen geometry, clamping methods, measurement devices and an assessment and improvement of data quality.

Click the attached report to review the Round Robin test program results and the Recommended Practice for Dynamic Tensile Testing for Sheet Steels.

Bookmark and Share

1 Comments
First  |  Previous  |  Next  |  Last
Be the first to comment on this article below!
First  |  Previous  |  Next  |  Last
Please sign in below to post a comment:
User Name:
Password:
 
Or, click here to create a FREE user account.